Differential scanning calorimeter DSC-800B

Short Description:

Differential scanning calorimeter DSC-800B   Summary: It can be tested for curing, glass transition temperature (tg), cooling crystallization, melting temperature and enthalpy variables, cross-linking degree, product stability, oxidation induction time (OIT) and other indicators. Conforming the following standards: GB/T 19466.2- 2009/ISO 11357-2:1999 GB/T 19466.3- 2009/ISO 11357-3:1999 GB/T 19466.6- 2009/ISO 11357-6:1999 Features: Industrial level widescreen touch structure is rich in infor...


  • FOB Price: US $0.5 - 9,999 / Set
  • Min.Order Quantity: 1 Set/Sets
  • Supply Ability: 10000 Set/Sets per Month
  • Port: QingDao
  • Payment Terms: L/C,D/A,D/P,T/T
  • Product Detail

    Product Tags

    Differential scanning calorimeter

    DSC-800B

     Differential scanning calorimeter DSC-800B

    Summary:

    It can be tested for curing, glass transition temperature (tg), cooling crystallization, melting temperature and enthalpy variables, cross-linking degree, product stability, oxidation induction time (OIT) and other indicators.

    Conforming the following standards:

    GB/T 19466.2- 2009/ISO 11357-2:1999

    GB/T 19466.3- 2009/ISO 11357-3:1999

    GB/T 19466.6- 2009/ISO 11357-6:1999

    Features:

    1. Industrial level widescreen touch structure is rich in information, including setting temperature, sample temperature, differential thermal signal, etc.
    2. USB communication interface, strong universality, reliable communication, support self-restoring connection function.
    3. The furnace structure is compact, and the rate of rising and cooling is adjustable.
    4. The installation process is improved, and the mechanical fixation method is adopted to completely avoid the contamination of the internal colloidal of the furnace to the differential heat signal.
    5. The furnace is heated by heating wire, compact structure and small size.
    6. The double temperature probe ensures the high repeatability of the sample temperature measurement, and adopts the special temperature control technology to control the temperature of the furnace wall to set the temperature of the sample.
    7. The gas flow meter automatically switches between two channels of gas, with fast switching speed and short stable time.
    8. Standard sample is provided for easy adjustment of temperature coefficient and enthalpy value coefficient.
    9. Software support each resolution screen, automatically adjust the computer screen size curve display mode. Support laptop, desktop; Support WIN7, WIN10, WIN11 and other operating systems.
    10. Support user edit device operation mode according to actual needs to achieve full automation of measurement steps. The software provides dozens of instructions, and users can flexibly combine and save each instruction according to their own measurement steps. Complex operations are reduced to one-click operations.

    Parameters:

    1. Temperature range: RT-800℃
    2. Temperature resolution:0.01℃
    3. Heating rate: 0.1~80℃/min  
    4. Temperature control mode: Heating, cooling, constant temperature, any combination of three modes cycle use, temperature uninterrupted
    5. DSC range: 0~±500mW
    6. DSC resolution: 0.01mW
    7. DSC sensitivity: 0.1mW
    8. Working power: AC 220V 50Hz 300W or other
    9. Atmosphere control gas: Two-channel gas control by automatic controlled (e.g. nitrogen and oxygen)
    10. Gas flow:0-200mL/min
    11. Gas pressure:0.2MPa
    12. Gas flow accuracy: 0.2mL/min
    13. Crucible: Aluminum crucible Φ6.5*3mm (Diameter * High),ceramic crucible Φ6.5*3mm (Diameter * High)
    14. Calibration standard: with standard material (Indium, tin, zinc, silver), users can adjust the temperature coefficient and enthalpy value coefficient by themselves
    15. Data interface: Standard USB interface
    16. Display mode: 7-inch touch screen
    17. Output mode: computer and printer

    Configuration list:

    1. DSC machine  1pc
    2. Aluminum crucible  300pcs
    3. Ceramic crucibles  50pcs
    4. Power cords   1pc
    5. USB cable   1pc
    6. CD (contains software and operations video)  1pc
    7. Software-key   1pc
    8. Oxygen tube  5m
    9. Nitrogen tube   5m
    10. Operation manual  1pc
    11. Standard sample (contains Indium, tin, zinc)  1set
    12. Tweezer   1pc
    13. Sample spoon    1pc
    14. Custom pressure reducing valve joint and quick joint  2 pair
    15. Fuse  4pcs

    Physical drawing:

       Aluminum crucibles

     

     

     

     

     

     

     

     

         Aluminum crucibles(Φ6.5*3mm)                   

     

    Ceramic crucible

     

     

     

     

     

     

     

     

    Ceramic crucible Φ6.5*3mm 

    Software screenshots: 

     

    DSC Sample Curve 1 DSC Sample Curve 2 DSC Sample Curve 3 DSC Sample Curve 4 

     


  • Previous:
  • Next:

  • SHANDONG DRICK INSTRUMENTS CO.,LTD

    Company Profile

    Shandong Drick Instruments Co., Ltd, is mainly engaged in the research and development, manufacturing and sales of testing instruments.

    The company established in 2004.

     

    Products are used in scientific research units, quality inspection institutions, universities, packaging, paper, printing, rubber and plastics, chemicals, food, pharmaceuticals, textiles, and other industries.
    Drick pays attention to talent cultivation and team building, adhering to the development concept of professionalism, dedication.pragmatism, and innovation.
    Adhering to the customer-oriented principle, solve the most urgent and practical needs of customers, and provide first-class solutions to customers with high-quality products and advanced technology.

  • Write your message here and send it to us

    Related Products

    WhatsApp Online Chat !